Original language | English |
---|---|
Pages (from-to) | 376-380 |
Journal | International Journal of Materials Research |
Volume | 4 |
Issue number | 99 |
DOIs | |
Publication status | Published - 2008 |
Treatment code (Nähere Zuordnung)
- Basic - Fundamental (Grundlagenforschung)
Christoph Stotter, Christof Sommitsch, Julian Wagner, Leitner Harald, Ilse Letofsky-Papst, Prantl Werner, Martin Stockinger, Gerald A. Zickler
Research output: Contribution to journal › Article › peer-review
Original language | English |
---|---|
Pages (from-to) | 376-380 |
Journal | International Journal of Materials Research |
Volume | 4 |
Issue number | 99 |
DOIs | |
Publication status | Published - 2008 |