Original language | English |
---|---|
Publication status | Published - 11 Apr 2011 |
Event | The 4th Symposium on Heat Resistant Steels and Alloys - Peking, China Duration: 11 Apr 2011 → 13 Apr 2011 |
Conference
Conference | The 4th Symposium on Heat Resistant Steels and Alloys |
---|---|
Country/Territory | China |
City | Peking |
Period | 11/04/11 → 13/04/11 |
Fields of Expertise
- Advanced Materials Science
Treatment code (Nähere Zuordnung)
- Basic - Fundamental (Grundlagenforschung)
- Experimental